ProzessTiangong LCADatensatzversion: v01.01.002

Jinfeng copper smelting process; Double-sided blowing melting pool smelting; Mixed production; In the factory [en]

Datenquelle: Tiangong LCA Data Working Group [en]

Referenzprodukt
copper matte [en]
Funktionelle Einheit
1000 kg
Region
Stadt Chifeng (Ulanhad), Autonomes Gebiet Innere Mongolei, China (CN-NM-CFS) · Geografische Genauigkeit nicht angegeben
Referenzjahr
2019

Datensatzbeschreibung

The raw material fed into the side-blowing melting pool during the smelting stage is copper concentrate, and quartz stone is used as the flux, with SiO2 content ≥95% and particle size ≤ 30mm. The energy sources invested are coke, electricity and natural gas. The oxygen introduced is prepared by the oxygen generation station and converted into electricity consumption. [Root-cause parallel repair (2026-11-18): D4:36d2ed1d->0ce3dedb] [en]

Technologiebeschreibung

The well-mixed copper smelting materials (flux, return material, fuel) are added from the top of the furnace, and at the same time, high-concentration (85-90%) oxygen-rich air is blown in. Under high temperature, about 97% of the iron in the materials is oxidized to form ferrous silicate slag, and about 85% of the sulfur is oxidized to SO₂ and enters the high-temperature flue gas (about 1250°C). [en]

Datensatz

Klassifikation
ILCD · C · Manufacturing; ILCD · 24 · Manufacture of basic metals; ILCD · 242 · Manufacture of basic precious and other non-ferrous metals; ILCD · 2420 · Manufacture of basic precious and other non-ferrous metals