ProcessTiangong LCADataset version: v01.01.001

Jinfeng copper smelting process; Rotary anode furnace refining; Mixed production; In the factory

Data source: Tiangong LCA Data Working Group

Reference product
Anode Plate
Functional unit
1000 kg
Geography
Chifeng(Ulanhad)Shi,Nei Mongol Zizhiqu,China (CN-NM-CFS) · Geographic precision not specified
Reference year
2019

Dataset description

The raw materials for the refining process of the anode furnace are fed into the crude copper continuously discharged from the blowing furnace, which flows continuously into the anode furnace through the chute. The energy input consists of electricity and natural gas, with natural gas serving as fuel and reducing agent.

Technology description

Crude copper continuously flows into the anode furnace. When the addition amount reaches approximately 150 tons (nearly two hours' output), air is blown in for oxidation operation (while continuing to increase the crude copper), causing residual sulfur to oxidize into SO₂ and enter the flue gas, and impurities to oxidize into slag and float up. After oxidation is completed, slag is discharged and immediately blown into a reducing agent for reduction. Once the endpoint is reached, casting is carried out. The entire feeding, oxidation, reduction and casting process requires the injection of natural gas and oxygen-rich air to maintain the temperature. The refined slag is slowly cooled and crushed before being returned to the smelting process. The flue gas is cooled by air dilution, through a plate cooler, bag filter and desulfurized by the limestone-gypsum method, and then discharged through the chimney.

Record

Classification
ILCD · C · Manufacturing; ILCD · 24 · Manufacture of basic metals; ILCD · 242 · Manufacture of basic precious and other non-ferrous metals; ILCD · 2420 · Manufacture of basic precious and other non-ferrous metals