Jinfeng copper smelting process; Double-sided blowing melting pool smelting; Mixed production; In the factory
Data source: Tiangong LCA Data Working Group
- Reference product
- copper matte
- Functional unit
- 1000 kg
- Geography
- Chifeng(Ulanhad)Shi,Nei Mongol Zizhiqu,China (CN-NM-CFS) · Geographic precision not specified
- Reference year
- 2019
Dataset description
The raw material fed into the side-blowing melting pool during the smelting stage is copper concentrate, and quartz stone is used as the flux, with SiO2 content ≥95% and particle size ≤ 30mm. The energy sources invested are coke, electricity and natural gas. The oxygen introduced is prepared by the oxygen generation station and converted into electricity consumption.
Technology description
The well-mixed copper smelting materials (flux, return material, fuel) are added from the top of the furnace, and at the same time, high-concentration (85-90%) oxygen-rich air is blown in. Under high temperature, about 97% of the iron in the materials is oxidized to form ferrous silicate slag, and about 85% of the sulfur is oxidized to SO₂ and enters the high-temperature flue gas (about 1250°C). The formed smelting slag is separated, slowly cooled and crushed, and then the copper concentrate is recovered by flotation and returned to smelting. The formed white ice copper is continuously discharged and flows into the blowing furnace. The high-temperature flue gas is treated with waste heat recovery and purification, and secondary air is used to ensure the combustion of individual sulfur in the flue.
Record
- Classification
- ILCD · C · Manufacturing; ILCD · 24 · Manufacture of basic metals; ILCD · 242 · Manufacture of basic precious and other non-ferrous metals; ILCD · 2420 · Manufacture of basic precious and other non-ferrous metals